Applications
This material is suitable for injection molding, profile extrusion and blown film extrusion.
Processing Recommendations
Extruder Zone Temperature F
Rear 300-329 F
Center 300-329 F
Front 300-329 F
Nozzle 300-329 F
Processing at temperatures above 350 F may result in combination of high shear condition such as high injection speed may result in thermal degradation of this resin.
GDH-B1 should be dried prior to processing
Drying Conditions:
Out of a sealed box: 90 to 100 F for 2-3 hours
Open box: 100 to 120 F for 4-5 hours
Specific recommendations for processing GDH-B1 can be made based on customer equipment and processes. For further suggestions, please contact Green Dot Holdings.